1、Specifications
(1)High brightening and perfect level in low area
(2)Easy to do the following Chrome plating without foggy
(3)Wide range of operating temperature
(4)Easy to control
(5)Use in both rack plating and barrel plating
2、Composition
Composition |
Standard |
Range |
Nickelous sulfate(NiSO4▪6H2O) |
280g/L |
250—300g/L |
Nickel chloride(NiCl2▪6H2O) |
55g/L |
50—60g/L |
Orthoboric acid(H3BO3) |
45g/L |
40—50g/L |
BNI-3A Throwing Agent |
6ml/L |
5—8ml/L |
BNI-3B Main Brightener |
0.4ml/L |
0.3—0.6ml/L |
Wetting agent NI-K (Cathode move NI-K) |
2ml/L |
1—3ml/L |
3、Basic consumption
The consumption is related to the electricity, the carry-out, the agitation way, the cleanness of the bath and surface condition of being plated parts.
BNI—3A Throwing Agent |
100--150 ml/1000AH |
BNI—3B Main Agent |
50--100ml/1000AH |
NI—K Wetting agent |
20--30 ml/1000AH |